Abstract
In their paper, Trtik et al. (2009) identify spurious peaks in the application of statistical nanoindentation technique as a critical obstacle for mechanical phase identification. In this discussion, we show that Trtik et al.'s finding is a consequence of an unrealistic virtual 3-D checkerboard microstructure considered by the authors. These peaks are not a general feature of indentation on multiphase materials, nor can the presence of such peaks be attributed to an intrinsic shortcoming of the grid-indentation technique. We also show that the authors' assertion of the absence of homogeneous material regions extending beyond 3 μm in cementitious materials is groundless.
| Original language | English |
|---|---|
| Pages (from-to) | 92-99 |
| Number of pages | 8 |
| Journal | Cement and Concrete Composites |
| Volume | 32 |
| Issue number | 1 |
| DOIs |
|
| Publication status | Published - 1 Jan 2010 |
| Externally published | Yes |
Keywords
- Microstructure
- Nanoindentation
- Statistical analysis
Fingerprint
Dive into the research topics of 'Does microstructure matter for statistical nanoindentation techniques?'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver