Résumé
Atomic Layer Deposition (ALD) of copper sulfide (CuxS) thin films from Cu(acac)2 (acac = acetylacetonate = 2,4-pentanedionate) and H2S as Cu and S precursors is reported. Typical self-saturated reactions ("ALD window") are obtained in the temperature range Tdep = 130-200 °C for an average growth per cycle (GR) = 0.25 Å/cycle. The morphology, crystallographic structure, chemical composition, electrical properties and optical band gap of thin films were investigated using scanning electronic microscopy (SEM), X-ray diffraction under Grazing Incidence conditions (GI-XRD), X-ray reflectivity (XRR), energy dispersive spectrometry (EDS), Hall effect measurements, and UV-vis spectroscopy. The obtained copper sulfide films are heavily p-doped (charge carrier concentration ~ 1021 -1022 cm- 3) with optical band gaps in the range of 2.2-2.5 eV for direct and 1.6-1.8 eV for indirect band gaps. Depending on the number of ALD cycles, multiphase compounds (made of digenite Cu1.8S, chalcocite Cu2S, djurleite Cu31S16 and covellite CuS) or single-phase digenite Cu1.8S films are obtained via a growth mechanism that involves in-situ copper reduction and loss of sulfur by evaporation.
| langue originale | Anglais |
|---|---|
| Pages (de - à) | 103-108 |
| Nombre de pages | 6 |
| journal | Thin Solid Films |
| Volume | 600 |
| Les DOIs | |
| état | Publié - 1 févr. 2016 |
Empreinte digitale
Examiner les sujets de recherche de « Atomic layer deposition of copper sulfide thin films ». Ensemble, ils forment une empreinte digitale unique.Contient cette citation
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver