Résumé
The occurrence of filaments in fused silica irradiated by UV laser light is well described by the product of light Intensity by Length of propagation in the material. For a spatially gaussian peak, in the well-known treatment by Marburger et al, this product is predicted to depend upon input power and non linear index. At a wavelength of 355 or 351 nm, the compilation of our past and present measurements give a smaller critical intensity by length product, i.e. a higher non linear index, than previously measured. These values of non linear parameters allow for the prediction of rear surface damage on thick windows. The predictions compare well with damage probability measurements. Even when the intensity is not high enough to generate filaments, self-focusing is still the cause of damage, due to the increase of output intensity and fluence.
| langue originale | Anglais |
|---|---|
| Numéro d'article | 37 |
| Pages (de - à) | 355-364 |
| Nombre de pages | 10 |
| journal | Proceedings of SPIE - The International Society for Optical Engineering |
| Volume | 5647 |
| Les DOIs | |
| état | Publié - 27 mai 2005 |
| Modification externe | Oui |
| Evénement | 36th Annual Boulder Damage Symposium Proceedings: Laser-Induced Damage in Optical Materials: 2004 - Boulder, CO, États-Unis Durée: 20 sept. 2004 → 22 sept. 2004 |
Empreinte digitale
Examiner les sujets de recherche de « Measurement and prediction of rear surface damage in fused silica windows caused by UV nanosecond pulses ». Ensemble, ils forment une empreinte digitale unique.Contient cette citation
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver