PWR effect on crack initiation under equi-biaxial loading development of the experiment

  • Université Paris-Saclay
  • Lamsid/EDF/R and D

Résultats de recherche: Contribution à un journalArticleRevue par des pairs

Résumé

The lifetime extension of the nuclear power stations is considered as an energy challenge worldwide. That is why, the risk analysis and the study of various effects of different factors that could potentially represent a hazard to a safe long term operation are necessary. The methodology for fatigue dimensions of the Pressurized Water Reactor components (PWR) is based on the use of design curves established from test carried out in air at 20 °C on smooth specimens by integrating safety coefficient that covers the dispersion of tests associated with the effects of structures. To formally integrate these effects, some international codes have already proposed and suggested a modification of the austenitic stainless steels fatigue curve combined with a calculation of an environmental penalty factor, namely Fen, which has to be multiplied by the usual fatigue usage factor. The aim of this paper is to present a new device "FABIME2E"developed in the CEA-LISN in collaboration with EDF and AREVA. These new tests allow quantifying accurately the effect of PWR environment on semi-structure specimen. This new device combines the structural effect like equi-biaxiality and mean strain and the environmental penalty effect with the use of PWR environment during the fatigue tests.

langue originaleAnglais
Numéro d'article619
journalMechanics and Industry
Volume20
Numéro de publication6
Les DOIs
étatPublié - 1 janv. 2019
Modification externeOui

Empreinte digitale

Examiner les sujets de recherche de « PWR effect on crack initiation under equi-biaxial loading development of the experiment ». Ensemble, ils forment une empreinte digitale unique.

Contient cette citation