TY - GEN
T1 - Residual stress measurements and modelling for temper bead qualification
AU - Ficquet, Xavier
AU - Robin, Vincent
AU - Kingston, Ed
AU - Courtin, Stéphan
AU - Yescas, Miguel
PY - 2013/12/1
Y1 - 2013/12/1
N2 - This paper presents results from a programme of through thickness residual stress measurements and finite element analysis (FEA) modelling carried out on a temper bead mock-up. Emphasis is placed on results comparison rather than the measurement technique and procedure, which is well documented in the accompanying references. Temper bead welding processes have been developed to simulate the tempering effect of post-weld heat treatment and are used to repair reactor pressure vessel components to alleviate the need for further heat-treatment. The Temper Bead Mock-up comprised of a rectangular block with dimension 960mm × 189mm × 124mm was manufactured from a ferritic steel forged block with an austenitic stainless steel buttering and a nickel alloy temper bead cladding. The temper bead and buttering surfaces were machined after welding. Biaxial residual stresses were measured at a number of locations using the standard Deep-Hole Drilling (DHD) and Incremental DHD (iDHD) techniques on the Temper Bead Mock-up and compared with FEA modelling results. An excellent correlation existed between the iDHD and the modelled results, and highlighted the need for the iDHD technique in order to account for plastic relaxation during the measurement process. Maximum tensile residual stresses through the thickness were observed near the austenitic stainless steel surface at 298MPa. High compressive stresses were observed within the ferritic base plate beneath the bimetallic interface between austenitic and ferritic steels with peak stresses of-377MPa in the longitudinal direction.
AB - This paper presents results from a programme of through thickness residual stress measurements and finite element analysis (FEA) modelling carried out on a temper bead mock-up. Emphasis is placed on results comparison rather than the measurement technique and procedure, which is well documented in the accompanying references. Temper bead welding processes have been developed to simulate the tempering effect of post-weld heat treatment and are used to repair reactor pressure vessel components to alleviate the need for further heat-treatment. The Temper Bead Mock-up comprised of a rectangular block with dimension 960mm × 189mm × 124mm was manufactured from a ferritic steel forged block with an austenitic stainless steel buttering and a nickel alloy temper bead cladding. The temper bead and buttering surfaces were machined after welding. Biaxial residual stresses were measured at a number of locations using the standard Deep-Hole Drilling (DHD) and Incremental DHD (iDHD) techniques on the Temper Bead Mock-up and compared with FEA modelling results. An excellent correlation existed between the iDHD and the modelled results, and highlighted the need for the iDHD technique in order to account for plastic relaxation during the measurement process. Maximum tensile residual stresses through the thickness were observed near the austenitic stainless steel surface at 298MPa. High compressive stresses were observed within the ferritic base plate beneath the bimetallic interface between austenitic and ferritic steels with peak stresses of-377MPa in the longitudinal direction.
UR - https://www.scopus.com/pages/publications/84894673380
U2 - 10.1115/PVP2013-97073
DO - 10.1115/PVP2013-97073
M3 - Conference contribution
AN - SCOPUS:84894673380
SN - 9780791855713
T3 - American Society of Mechanical Engineers, Pressure Vessels and Piping Division (Publication) PVP
BT - ASME 2013 Pressure Vessels and Piping Conference, PVP 2013
T2 - ASME 2013 Pressure Vessels and Piping Conference, PVP 2013
Y2 - 14 July 2013 through 18 July 2013
ER -