Very slow creep tests on rock samples

  • P. Bérest
  • , J. F. Béraud
  • , M. Bourcier
  • , A. Dimanov
  • , H. Gharbi
  • , B. Brouard
  • , K. Devries
  • , D. Tribout
  • Department of Mechanics École Polytechnique
  • Brouard Consulting
  • RESPEC
  • Compagnie des Salins du Midi et Salines de l’Est

Résultats de recherche: Le chapitre dans un livre, un rapport, une anthologie ou une collectionChapitreRevue par des pairs

1 Citation (Scopus)

Résumé

Twelve years ago, creep tests at very low deviatoric stress were performed on an Etrez salt sample in the Varangeville Mine. Recently, a new testing campaign was performed on various salt samples to gain further insight on salt behavior. Creep tests are performed under a 0.1 MPa uniaxial loading on rock-salt samples from the Varangeville and Avery Island Mines and under a 0.24 MPa uniaxial loading on a crushed-salt sample. To minimize the effects of temperature variations, testing devices were placed in an underground mine room, where temperature fluctuations are of the order of one-hundredth of a degree Celsius. The mechanical loading is provided by dead weights. The deformations were measured through special displacement sensors with a resolution of 1/80 μm. A typical steady-state strain rate reached after 6 months is −2.4 × 10−12 s−1. The influence of air hygrometry, which is approximately 74% RH in the mine, is smaller than expected.

langue originaleAnglais
titreMechanical Behaviour of Salt VII
EditeurCRC Press
Pages81-88
Nombre de pages8
ISBN (Electronique)9780203100769
ISBN (imprimé)9780415621229
étatPublié - 1 janv. 2012
Modification externeOui